When a marble adhesive repair cracks again, locate the new opening before choosing another filler. The opening may run through the repair material, along its edge or into the surrounding stone. Each observation points to a different investigation.
Then establish when it appeared: during finishing, after handling or after the piece entered service. Connect that timing with the product, preparation, mixing and support records.
This guide addresses the review of local fabrication repairs. Where damaged stone is unstable or its integrity affects safe handling or installation, have the component and assembly assessed before further repair work. A neat surface fill does not establish that the whole piece is sound.
1. Confirm What Has Changed Since the Repair
Compare the current condition with photographs taken before repair and after finishing. Identify whether the reported line is new, has extended or has simply become more visible under different lighting.
Separate an open line from a color difference, a shallow depression or a remaining scratch. Record what is visible rather than calling every mark a new crack. Similar-looking lines can require different follow-up.
Take an overall view that locates the repair and a close-up that shows its boundaries. Keep the stone orientation, lighting and photograph references identifiable. Include an accessible edge or underside where it helps show the condition without moving or disturbing unstable material.
KEDA’s stone fabrication and repair guidance distinguishes local defects, joints and edge assembly. State which of those tasks was performed, along with the original damage and the intended finished result.
Preserve the condition before refilling, polishing or applying another treatment. Once the surface is covered again, useful evidence about the opening and previous repair may be lost.
2. Locate the Opening Relative to the Repair
Describe the visible path in relation to the fill and stone. Use the following table to organize observations, not to assign a cause from one photograph.
| Visible observation | What to record | Next question |
|---|---|---|
| Opening within the filled region | Position, extent and appearance of the surrounding fill | What material and process produced that region? |
| Opening along a repair boundary | Which edge is affected and any visible separation | What surface and existing material did the fill contact? |
| New line extending into stone | Direction and connection with the original defect | Does the stone and its support need further assessment? |
| A piece of fill has become loose | Original position and corresponding exposed area | What surfaces and material remain at the separation? |
| Visible line without an established opening | Lighting, finish and comparison with earlier photographs | Is this cracking, an appearance difference or another surface condition? |
Keep detached material identified if it can be retained safely. Photograph corresponding surfaces before cleaning them. Describe residue and location without assuming that a clean-looking face proves contamination or that stone fracture proves universal adhesive strength.
Where the path is unclear, record that uncertainty and seek inspection. Applying pressure, bending the piece or prying open a line would change the condition being investigated.

Fictional opening-location illustration, not an actual KEDA failure specimen or a diagnosis of its cause.
3. Check Whether the Selected Product Fits the Repair
Identify the full product name, supplied grade, components and any permitted additions. Confirm that the original choice addressed the defect and application, rather than only matching the stone color.
Adesivo de poliéster tipo mármore KEDA para facas is a discussion point for suitable nonstructural fabrication and local repair. A paste applied to the surface should not be assumed to have reached the full depth of a narrow or through-body defect.
Ask what the repair was expected to achieve. Filling a small cosmetic cavity and restoring the integrity of a damaged stone component are different decisions. Crack depth, access and the condition of the whole piece belong in that review.
For a designated installation interface, KEDA 2-Component Epoxy Structural Adhesive is a separate product discussion. Its name does not make it an automatic replacement filler for every cracked stone repair.
The International Masonry Institute’s stone-restoration guidance connects crack-repair selection with crack stability and the condition of the stone unit. Apply that principle by establishing the repair task first. Repeatedly changing resin families leaves an unresolved defect or assembly problem unresolved.
4. Review the Surfaces the Repair Actually Contacted
Record how the original repair area was prepared and what material remained there. Include stone dust, earlier filler, surface treatment and any cleaner used in the process. Identify the actual contact surfaces rather than describing only the polished face beside them.
Check the preparation against the selected product’s instructions. Confirm the required surface condition and the method used to achieve it. If cleanliness or dryness was assumed rather than checked, make that gap visible in the record.
For repeat work, obtain a removal and preparation plan before disturbing the old repair. The plan should identify which material is unsound, which surfaces need to be exposed and how the surrounding finish will be protected.
Avoid treating a thin new cover as a solution to an unidentified underlying problem. Likewise, do not use an arbitrary groove, aggressive solvent or heating method simply because it was demonstrated on a different product or stone.
Keep the prepared area identifiable during a representative trial. Photograph it before filling and record the actual method, so a later result can be connected to the preparation that produced it.
5. Reconstruct Component Measurement and Mixing
Review the actual quantities and measurement basis used. Confirm the matched curing component, mixing method, batch conditions and any color-paste addition. A remembered description such as “the usual amount” provides little basis for comparison.
For polyester marble adhesive, use the hardener instruction for the supplied grade. Extra hardener is not a general treatment for a repair that has opened, and a tinting accessory does not replace the curing component.
If the specified KEDA structural epoxy was used, its A:B ratio is 1:1 by volume. Equal weights are not an established substitute. Keep that instruction attached to the actual product; it does not define the ratio of another epoxy or a polyester repair adhesive.
Record whether the mixture was applied within its permitted working stage and whether components or additives were changed during use. Keep the facts about the affected preparation separate from later attempts to make a different mixture.
Where the record is incomplete, state what is missing. An accurately prepared comparison can help investigate a process question, but it cannot retrospectively establish how the original batch was made.
6. Connect the New Opening with the Operation Before It
Build a timeline from preparation to the first observed change. Timing helps focus the review, although it does not establish the cause on its own.
| When the change was first noticed | Record the preceding operation | Point to review |
|---|---|---|
| Before machining | Mixing, application, positioning and curing conditions | Material preparation and permitted processing stage |
| During sanding or polishing | Operation, tool, process and elapsed time | Readiness for that operation and the affected detail |
| After lifting or transport | Handling sequence, restraint and support arrangement | Whether handling and component condition need assessment |
| After installation or use | Installation history, service events and observed changes | The component, receiving system and actual exposure |
| Timing unknown | Last documented acceptable condition and first current record | What history can still be reconstructed? |
Keep handling, machining and service release separate where the instructions distinguish them. Surface hardness or an attractive polished finish does not define readiness for every subsequent operation.
If measured bond evidence is needed, agree the relevant evaluation separately. KEDA’s guide to testing stone adhesive bonds explains why specimen, method, cure and failure location must remain connected. An informal observation during workshop use is different from a controlled test result.
7. Review the Whole Piece and Its Support History
Include the original defect location, component shape and support or attachment arrangement in the inquiry. For installed work, ask the responsible installer or assessor to review the relevant assembly, rather than limiting the discussion to the visible filler.
Record reported events such as impact, relocation, alteration or a change in use. Identify where those facts came from. Avoid assigning a cause simply because an event occurred before the opening was noticed.
If movement or an unresolved installation condition is suspected, have it assessed before repeating a rigid local fill. A moving crack and a stable cosmetic defect require different repair decisions. Substituting a flexible sealant without that assessment would also leave the component’s condition unresolved.
Ask for a broader inspection where new damage extends beyond the repaired area, an attached piece is loose or the stone’s stability is uncertain. The assessment may change the proposed work from local filling to another repair strategy or replacement.
Retain the specified supports and fixings during that review. This guide does not establish bracket positions, anchor quantities, load capacity or a method for testing an installed piece by hand.

Fictional observation scene. The continuous bench support is not an installation design or a statement that damaged stone is safe.
If an opening follows a support line or returns after the piece is moved, document the location of the supports before planning another fill. The Natural Stone Institute's Dimension Stone Design Manual is a reference for reviewing the surrounding stone assembly with the project team.
8. Define What Will Change Before Trying the Repair Again
Turn the investigation into a written next step. Identify the unresolved question, the proposed change and the evidence needed before returning the work to its intended use.
| Finding from the review | Action to define | Evidence to keep |
|---|---|---|
| Product selection does not match the task | Review the defect and suitable repair approach | Confirmed scope and product instructions |
| Contact surface or preparation is unclear | Establish an appropriate preparation method | Identified surfaces and preparation record |
| Measurement or mixing departed from instructions | Correct the specific preparation step | Actual amounts, basis and mixing record |
| Change appeared during a later operation | Review readiness and the operation performed | Timing, process and subsequent inspection |
| Stone stability or support remains unresolved | Refer the component and assembly for assessment | Assessor’s findings and defined next work |
For a suitable nonstructural trial, use representative stone and the confirmed method. KEDA’s sample-evaluation guide provides a way to record preparation, processing and finished results.
Change the relevant variable deliberately and preserve the earlier observation. Replacing the stone, adhesive, tint and finishing method together makes it difficult to learn which change mattered.
Separate appearance acceptance from any required performance or assembly assessment. A neat trial patch answers the appearance question under its trial conditions; record the additional decisions that remain open.
9. Send a Focused Repair-History Record
Provide the original defect, exact product and components, previous repair attempts and the current opening location. Add the timeline, preparation and mixing records, finishing operations, service conditions and relevant support information.
Number the photographs and include an overall view alongside the detail. Mark which condition each image records. Preserve original images so the reviewer can distinguish observations from later annotations.
A useful question is: “The opening first appeared along one repair edge after polishing. Here are the original defect, preparation, mix record and processing timeline. Which product or process information should we verify before repeating the repair?”
Use the troubleshooting record with the crack path, nearby supports and the date the crack returned.
Entre em contato com a KEDA with that record for a product-related review. Where the issue concerns the stone component or installation, include the responsible fabricator or project assessor so the next action addresses the actual problem.

Blank editorial record props, not an actual case file, diagnostic report or repair approval.
Perguntas frequentes
1. Does a new crack prove the adhesive is defective?
No. Locate the opening and review material, preparation, processing and component history. The observation needs investigation before a cause can be assigned.
2. Should we use a stronger epoxy immediately?
First define the defect and repair purpose. A different product needs its own selection and evaluation; it does not resolve an unidentified support or stability problem.
3. Can we fill directly over the old repair?
Obtain an appropriate removal and preparation plan for the actual condition. Covering the surface alone does not address unsound material or an unresolved cause beneath it.
4. What if the repair looked good before polishing?
Record when the change appeared and the operation performed. Review the permitted processing stage and method rather than judging readiness from appearance or surface hardness alone.
5. Can a small trial establish that the whole piece is safe?
No. It supports the question evaluated on that specimen. A damaged component’s handling, support and installation suitability require the relevant assessment of the whole piece and assembly.