“The glue failed” describes a concern, but leaves the supplier with several unanswered questions. Was the adhesive still soft, did a joint separate, or did the finished repair change appearance? Which components were used, and what happened before the problem appeared?
Useful stone adhesive troubleshooting starts with a clear record of the product, materials, process and observed condition. A concise case summary, readable labels and a coordinated photo set help the customer, distributor and supplier discuss the same event.
Use this guide to prepare that first support submission and keep subsequent findings organized.
1. Describe the Observed Problem and Its Extent
Start with what someone actually saw. Write “the edge strip separated during polishing” or “the repair remained soft at the recorded inspection time.” These descriptions identify an event without assigning a cause prematurely.
Record the application, discovery date and current condition. Include the number of affected pieces and the total number checked, using the same counting unit. Three affected joints among twelve inspected joints is more informative than “some customers have problems.”
| Customer description | Information to record first | Useful supporting record |
|---|---|---|
| Adhesive remains soft | Where it is soft and when it was inspected | Mixing details, application time and actual conditions |
| Joint separated | Operation or event when separation appeared | Overall assembly and accessible separated faces |
| Repair sank or developed holes | Appearance before and after finishing | Dated photographs and finishing sequence |
| Seam changed color | When and where the change became visible | Comparable photographs, stone treatment and exposure history |
| Material looked unusual in its pack | Component, unopened or opened state, and discovery | Original label and container-condition photographs |
Note whether the affected pieces came from one mixing batch, one container or several containers. Keep uninspected work separate from the confirmed count.
When several symptoms occur together, list each one with its discovery time. A dark seam noticed before polishing and an edge separation noticed afterward are two observations to connect through the timeline, rather than one combined claim with an assumed explanation.
For installed stone that may be unstable, restrict access and involve the responsible installer or project professional before approaching, moving or loading it. Document only from a safe position. The evidence-gathering steps below do not require pulling an installed joint apart.
2. Identify the Product and Every Curing Component
Photograph the original product label, grade, color, capacity and any visible lot or date markings. Record the order reference and where the material was obtained. Include the matched hardener or second component, with its own markings where present.
For KEDA’s Knife Grade Polyester Marble Adhesive, identify the supplied hardener and the dose actually used. State the measurement method and any color paste addition. The accessory, base adhesive and curing component should remain distinguishable in the record.
For the specified KEDA 2-Component Epoxy Structural Adhesive, the confirmed A:B instruction is 1:1 by volume. Record whether the operator measured volumes or weights; equal weights do not establish equal volumes.
Copy label markings exactly. If a code is unclear, attach its photograph rather than guessing whether it is a production date, expiry date or lot identifier. If material was decanted, document the original container and transfer history when available.
Also record receipt, first opening and storage history. Separate a measured temperature from a recollection such as “the warehouse was warm.” Unknown fields can stay explicitly unknown.

Fictional containers illustrate identity fields to record; they are not KEDA packaging or a mixing-ratio guide.
3. Describe Both Bonding Faces and the Assembly
Give the stone name or supplier designation, finish and any known resin, mesh, sealer or other treatment on the bonding face. “Marble” alone does not describe a treated stone back or a polished edge.
Identify the adjoining material just as carefully. For metal, include its known coating or finish. For another stone piece, describe that piece’s bonding surface too. Record the joint arrangement, accessible dimensions, support and intended use.
Explain surface preparation in sequence: what was removed, which tools and products were used, and what happened before adhesive application. Write the actual process rather than replacing it with “prepared correctly.” Keep the cleaner’s identity when known.
KEDA’s stone fabrication and repair guidance provides context for joints, fabricated edges and local repairs. Use the specific operation in the case description so a filling issue is not discussed as though it were a stone-to-support installation.
Distinguish measurements taken before bonding from dimensions estimated after separation. Mark inaccessible information accordingly.
4. Reconstruct the Mixing-to-Discovery Timeline
Record the component amounts, ratio basis, mixing method, batch quantity and container used. Note any pigment, filler, solvent or other addition, including its identity and amount if known. An accurate record of a deviation is more useful than an idealized procedure.
Build the sequence around mixing, application, positioning, support removal, machining and discovery. Use actual dates and times where available, with a time zone for teams working internationally. Identify estimates as estimates.
Include relevant temperature readings, where they were taken and when. Air, stone and stored adhesive may have different histories. If the workshop did not measure them, report that gap instead of inserting a weather-app value as a substrate measurement.
Record events after application, including relocation, polishing, water exposure, cleaning or loading. These events establish the sequence; their presence alone does not prove a cause.
A hardened remainder in the mixing container is worth documenting, but its condition does not establish that an installed joint followed the same curing history. Keep the two observations separate.

Blank recording prompts. Enter the actual process times; these cards do not specify a curing schedule.
5. Take a Photo Set That Answers Different Questions
Begin with an overall view, then move closer. A sharp close-up can show a surface condition while hiding the joint’s location, support or surrounding material. The wider photograph supplies that context.
| Photograph | What to include | Practical detail |
|---|---|---|
| Overall view | Affected piece and surrounding assembly | Identify the joint in a separate annotated copy |
| Joint detail | Visible seam, repair or defect | Focus on the surface, with steady neutral lighting |
| Accessible separated faces | Both corresponding sides, if already separated | Preserve orientation and identify each face |
| Product and components | Full readable labels and relevant markings | Photograph each supplied component separately |
| Comparison area | A nearby unaffected area or comparable piece | State exactly what makes it comparable |
| Process evidence | Existing mixing, support or finishing records | Label when the photograph was taken |
Retain the original files. Send annotated copies alongside them when arrows or circles help locate the issue. Avoid filters, color enhancement and excessive compression, especially for color complaints.
For a safely accessible small workshop sample, a scale reference in the same plane can help communicate visible size. Record critical dimensions separately; perspective can distort photographic measurements.
Name files consistently, such as case-overview, joint-detail and label-component-1. Put the same identifiers in the written summary. A short video can supplement the photographs when motion matters, without deliberately stressing or demonstrating failure of an installed assembly.

Staged editorial views illustrate framing. They are not photographs from a customer complaint or evidence of a defect.
6. Record the Separation Location Without Guessing the Cause
If pieces have already separated and are safe to examine, photograph both corresponding faces before cleaning them. Describe where adhesive, stone, coating or backing remains visible. Keep the orientation and pairing clear.
Adhesive-bond analysis distinguishes separation at an interface, within adhesive, within a substrate and combinations of these locations. A coating or backing layer can also be part of the observed separation path. These categories organize observations; a photograph may not resolve the exact boundary.
Use plain descriptions such as “pale material remains on both faces” or “mesh is visible on one side.” Reserve a definite failure-mode classification for an adequately supported assessment.
An apparently clean face does not establish that the product was defective, and broken stone does not by itself approve the complete assembly. Strength, suitability and responsibility require more context than the appearance of one fragment.
If evaluation is needed, KEDA’s guide to testing stone adhesive bonds explains how specimen, method and failure-location records support interpretation. Agree the question and method before arranging further testing.
7. Preserve Relevant Material Before Altering the Evidence
Once the area is made safe, avoid cleaning, grinding or rebonding accessible evidence before documenting its condition. If urgent work must proceed, record what was changed, when and by whom.
Keep original labels and relevant order records. Ask the supplier what retained material would be useful before collecting, cutting or returning samples. Handling, suitable containers, identification and shipment depend on the actual materials and their safety information.
Keep components separate and identified. Do not combine residues or mix a fresh batch simply to include it in a parcel. Confirm return arrangements and carrier requirements before shipping chemicals or contaminated pieces.
Record who retained each item and where it is stored. This maintains a usable connection between photographs, material and the reported event without turning an informal collection into a claimed laboratory investigation.
8. Send One Organized Case Summary
Give the distributor and supplier one case reference and a designated contact. A short summary followed by labeled attachments is easier to review than scattered messages from several people.
Keep the customer’s original description alongside any translation. Clarify workshop terms such as “dry,” “set” or “broken” by asking what operation or visible condition the speaker means. Preserve that clarification in the shared record.
| Case-summary field | What to enter |
|---|---|
| Product and supply | Grade, components, markings and order reference |
| Application | Both bonding faces, treatment, joint and intended use |
| Observed issue | Condition, discovery event and affected versus inspected quantity |
| Process history | Actual preparation, ratio basis, mixing and timed operations |
| Evidence | Original photographs, relevant records and retained items |
| Information gaps | Missing measurements or details awaiting confirmation |
| Requested next step | Clarification, evidence review or agreement on further evaluation |
Open with a direct request: “Please review the attached record and confirm what additional information is needed before a representative evaluation is arranged.” Add the operational deadline and current work status without presenting the deadline as a promised response time.
Separate technical questions from commercial requests such as replacement or credit. Record both, while allowing the technical review to establish what the available evidence supports. The summary itself does not determine warranty coverage or liability.
ASQ's check sheet guide gives a simple way to record recurring observations in the same format. Keep one line per affected piece or batch so the supplier can compare the defect location, time of discovery and material lot.
9. Close the Case with a Defined Next Action
After the first response, list the outstanding questions, responsible person and next review date. Add new findings to the existing case rather than creating parallel versions with conflicting descriptions.
When a controlled trial is agreed, record the materials, process, acceptance criteria and reviewer. Keep the trial findings distinct from the original complaint and document any changed variable. A proposed adjustment should become a confirmed instruction before routine production adopts it.
KEDA’s distributor and partner information outlines the cooperation context. For a specific product issue, contact KEDA with the case summary and available evidence, then confirm the appropriate review and next steps.
Frequently Asked Questions
1. What should I send first if the adhesive is not curing?
Send the product and curing-component labels, actual amounts and measurement basis, mixing and application times, observed condition and available temperature records. Identify whether the observation concerns material in a container, the joint or both.
2. Can a photograph prove why a stone joint failed?
A photograph can show location and appearance. Determining cause may also require process records, material identification and an agreed evaluation. Include both accessible faces and the assembly context rather than relying on one close-up.
3. Should I clean the separated surfaces before photographing them?
Photograph accessible surfaces in their existing condition first, once safe. Cleaning or abrasion can remove useful evidence. Record any treatment already performed and ask what retained samples are needed before changing them further.
4. What if the lot marking or workshop temperature is missing?
State that it is unavailable. Supply the readable label photographs, order details and known history. Keep an estimate clearly labeled; an invented code or measurement can misdirect the review.
5. Does reporting several failures establish a defective batch?
Report the affected and inspected quantities, container references and application history. A shared lot is a useful lead, but shared materials or processes also need review. Keep the batch conclusion open until the evidence supports it.
| What you observed | Where to start |
| — | — |
| Soft, sticky or uneven cure | Check mixing, hardener and cure conditions |
| The working time is too short | Check why marble adhesive is setting too fast |
| Paste will not spread or hold its shape | Check excessive thickness or runniness |
| Separation, skin or lumps in the container | Check the container and storage history |
| A cured repair sits below the stone | Investigate shrinkage and a sunken repair |
| Voids or pinholes show after finishing | Trace air, mixing or voids in the repair |
| A repaired crack returns | Investigate movement and repeat cracking |
| A seam turns yellow or dark | Compare discoloration and the surrounding stone |
| Residue remains beside the joint | Separate fresh smears from cured excess |